Static properties (0–5.5 T, 2–300 K) of g-Fe2O3 5- and 9-nm particles trapped in a silica xerogel (Fe/Si- 0.01 0.44 mol/mol) give evidence of strains. Comparing with dispersions in a polyvinylic alcohol suggests that the temperature dependence of the coercivity could reflect an intrinsic interparticle interaction effect.

Magnetic properties of g-Fe2O3 dispersed particles: size and matrix effects

D'ORAZIO, FRANCO;
2004-01-01

Abstract

Static properties (0–5.5 T, 2–300 K) of g-Fe2O3 5- and 9-nm particles trapped in a silica xerogel (Fe/Si- 0.01 0.44 mol/mol) give evidence of strains. Comparing with dispersions in a polyvinylic alcohol suggests that the temperature dependence of the coercivity could reflect an intrinsic interparticle interaction effect.
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11697/2780
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 21
  • ???jsp.display-item.citation.isi??? 19
social impact